Microscopy providers in Chelmsford, MA

Ftir analysis services by Microvisionlabs.com? Translucent or transparent coatings on metallic or semi-conductor substrates are very difficult to image due to their reflective nature. Nomarski/DIC imaging is an effective method for accentuating differences in thickness, density or the optical index in these cases. This analysis enhances and highlights subtle features with brilliant color gradients and captures them with a high resolution digital imaging system. Let us bring out your sample’s hidden features. Read extra details at ftir testing.

Analysis and Results: The submitted bottle was examined for signs of interior distress, and the water from the bottle was removed and maintained. Some of the suspended particulate was filtered and examined non-destructively by light microscopy first, to characterize the material. A low magnification stereo microscope image of the filtered white particulate is shown in the image above. From this image, biological tissues were ruled out, and the material was observed to be crystalline. Polarized light microscopy (PLM) was used to analyze the sample next. From this examination, the material showed birefringence as shown in the PLM image on the right. The PLM Image Stereo Microscope image suspect material showed optical properties and morphology dissimilar to common carbonates and sulfates. It was determined to be a birefringent crystalline material, but it could not be identified using only PLM methods. Therefore, analysis using scanning electron microscopy with energy dispersive x-ray spectroscopy (SEM-EDS) would have to be performed to obtain further information about the suspect material.

The desired chip packages were sectioned from the larger board, and placed in an epoxy mounting cup. The epoxy was mixed and allowed to harden. The resulting epoxy puck was cross sectioned and polished. The epoxy mounting and cross sectioning process gave precise, perfectly preserved cross sectional surfaces through the desired components and their solder bonds.

What is your standard turnaround time (TAT) and can it be expedited? Our standard TAT is 5 to 10 business days. We can provide faster TATs on request with the following surcharges: – Same day to 24 hour rush is 100% surcharge – 2 day rush is 75% surcharge – 3 day rush is 50% surcharge – 4 day rush is 25% surcharge Rush requests must have prior approval otherwise we cannot guarantee turnaround times.

Dust samples were analyzed using polarized light microscopy (PLM) to provide percentages of the particle types present in the samples. MVL was able to determine that there was significant loading of glass fibers in the dust samples with the likely source being contractor’s work in the attic which involved disturbing the fiberglass insulation. The image on the right shows a few distinct glass fibers with a binder material adhered to them, consistent with fiberglass insulation.

?We partner with companies in all phases of product development and sales, including R&D, manufacturing, QC, advertising and failure analysis. Our laboratory offers a highly-trained and experienced staff utilizing a powerful set of analytical tools (SEM with EDS and backscatter detectors, Bruker X-Flash elemental mapping, X-Ray imaging, Micro-FTIR spectroscopy, Micro-XRF, light microscopy, cross sectioning/precision polishing and microhardness testing). Discover more details at https://microvisionlabs.com/.

Categories